CHIPQUIK 50g Jar Solder Paste

  • RS Stock No. 146-6191
  • Mfr. Part No. SMD291AX50T3
  • Manufacturer CHIPQUIK
Technical data sheets
Legislation and Compliance
Non Compliant
COO (Country of Origin): CA
Product Details

Solder Paste in jar 50g (T3) Sn63/Pb37 no clean 90.25% metal.

Printing speeds up to 100mm/sec
Long stencil life
Wide process window
Clear residue
Low voiding
Excellent wetting compatibility on most board finishes
Print grade
Compatible with enclosed print heads
Passes BONO test

Specifications
Attribute Value
Package Type Jar
Package Size 50g
7 Within 4 working day(s)
109 Within 6 working day(s) (Global stock)
Price Each
PHP 900.31
(exc. VAT)
PHP 1,008.35
(inc. VAT)
units
Per Unit
1 - 9
PHP900.31
10 - 19
PHP875.50
20 - 49
PHP855.89
50 +
PHP804.38
Related Products
Tack Flux no clean in a 10cc syringe ...
Description:
Tack Flux no clean in a 10cc syringe w/plunger & tip. Used for touch up and rework, attachment of BGA spheres, soldering flip chip components. Low viscosity no-clean synthetic paste flux. Has a pleasant odor. Ideal for all rework, solder, ...
Tack Flux no clean 5cc (for lead-free applications) ...
Description:
Tack Flux no clean 5cc (for lead-free applications) w/plunger & tip. Low viscosity no-clean synthetic paste flux. Has a pleasant odor. Ideal for all rework, solder, de-solder and reflow applicationsNon-corrosive, non-conductive, no-cleanTack flux will not run all over PCB when ...
Tack Flux supplied in 6 2cc Squeeze Tubes ...
Description:
Tack Flux supplied in 6 2cc Squeeze Tubes (same flux as SMD291). Low viscosity no-clean synthetic paste flux. Has a pleasant odor. Ideal for all rework, solder, de-solder and reflow applications Non-corrosive, non-conductive, no-clean Tack flux will not run all ...
Tack Flux in 8cc Squeeze Tube (same flux ...
Description:
Tack Flux in 8cc Squeeze Tube (same flux as SMD291). Low viscosity no-clean synthetic paste flux. Has a pleasant odor. Ideal for all rework, solder, de-solder and reflow applicationsNon-corrosive, non-conductive, no-cleanTack flux will not run all over PCB when appliedHas ...